EN 10269 Grade X6CrNiTiB18-10 / 1.4941
EN 10269 Grade X6CrNiTiB18-10 / 1.4941
This European Standard specifies requirements for semi-finished products, bars and rods for fasteners with
properties specified at elevated and/or low temperatures made of non-alloy and alloy (including stainless)
steels and nickel alloys as given in Table 1.
The requirements of this standard may be applied also to the finished fasteners.
The general technical delivery conditions in EN 10021 also apply to products supplied in accordance with this
European Standard.
Grade X6CrNiTiB18-10 Chemical Composition
Material designation |
Chemical composition, % by mass |
Element |
Number |
C |
Si |
Mn |
P max. |
S max. |
Altot |
B |
Cr |
Mo |
Ni |
V |
Others |
X6CrNiMoB17-12-2 |
1.4919 |
0,04 to 0,08 |
≤ 1,00 |
≤ 2,00 |
0,035 |
0,015 |
– |
0,001 5 to 0,005 0 |
16,5 to 18,5 |
2,00 to 2,50 |
10,0 to 13,0 |
– |
N ≤ 0,10 |
Grade X6CrNiTiB18-10 Mechanical Properties
Material designation |
Heat treatment condition a |
Diameter c (d mm) |
Proof strength (Rp0,2 MPa min.) |
Tensile strength (Rm MPa) |
Elongation after fracture (A % min) |
Reduction in area (Z % min) |
Impact energy (ISO-V) at 20 °C (KV2 J min) |
Name |
Number |
X6CrNiMoB17-12-2 |
1.4919 |
+AT |
d ≤ 160 |
205 |
490 to 690 |
35 |
– |
100 |